Ihe ọmụma gbasara ịgbado ọkụ laser Isiokwu nke abụọ: Ịgbado ọkụ laser - njikwa ntụpọ

 

Dịka ngwa ọrụ nhazi dị elu, laser na-arụ ọrụ dị mkpa n'ọhịa nke ịgbado ọkụ ụlọ ọrụ mmepụta ihe. Ọ bụ ezie na teknụzụ ịgbado ọkụ laser ọdịnala nwere ike ijikwa ntụpọ ndị a ruo n'ókè ụfọdụ, mmetụta ya na-abụkarị site na paramita na usoro ịgbado ọkụ edobere. N'afọ ndị na-adịbeghị anya, ọdịdị nke teknụzụ ịgbado ọkụ laser na-enye ngwọta ọhụrụ maka njikwa ntụpọ ịgbado ọkụ. Site na iwebata ịgbado ọkụ laser n'oge usoro ịgbado ọkụ, teknụzụ ahụ nwere ike imeziwanye njirimara ike nke ọdọ mmiri ịgbado ọkụ nke ukwuu, si otú a na-eme ka mma ịgbado ọkụ dịkwuo mma. Teknụzụ ịgbado ọkụ laser dabere na njikwa ziri ezi nke teknụzụ ịgbado ọkụ laser na ịgbado ọkụ iji nweta ịgbado ọkụ dị irè na nke dị elu.

Meziwanye ọdịdị:

N'oge ahụusoro ịgbado ọkụ, a na-atụgharị ogwe laser ahụ ngwa ngwa na nke ziri ezi iji kpuchie mpaghara njikọta ahụ dum. Mgbe ogwe ahụ na-agagharị n'akụkụ njikọ ahụ, ọ na-agbagharị n'ụdị dị iche iche, dị ka okirikiri, eserese 8 na helix. Chen na ndị otu ya jiri laser swing iji wedata alloys aluminom dị iche iche, ma e jiri ya tụnyere enweghị ịgbado ọkụ laser swing, ọdịdị weld n'ihu na azụ nke ịgbado ọkụ laser swing ka mma nke ukwuu. Na mgbakwunye, a na-eji ịgbado ọkụ laser transverse swing iji mee ka mgbanwe nke oghere ahụ dịkwuo mma. Na ụfọdụ ọrụ njikọ conductive, ọ dị mkpa ịgbasa mpaghara overcurrent, ọ dịkwa mkpa ịgbasa elu njikọ metal, ọ dịkwa mkpa ịgbado ọkụ laser iji mee ka elu njikọ metal ghọọ "U".

Ịgbado ọkụ laser

1. (a) na (b) ọnụọgụgụ nke nhazi akụkụ cross na nha weld n'okpuru ụdị swing dị iche iche; (c) Ịmepụta elu elu nke weld n'okpuru ụdị swing dị iche iche.

Meziwanye njikọ mgbidi dị n'akụkụ adịghị mma:

Nrụgide nke enweghị njikọ mgbidi dị n'akụkụ dị mfe ime na njikọta laser dị warara nke efere dị ọkara dị arọ, nke na-akpata nkesa na-adịghị mma nke ike laser n'ọnụ, ntinye okpomọkụ dị n'etiti oghere ahụ buru ibu, ntinye okpomọkụ dị na mgbidi akụkụ nke oghere ahụ dịkwa obere, nke na-enweghị ike ịmepụta ezigbo njikọta. Isi ihe dị mkpa iji dozie ntụpọ mgbidi akụkụ na-adịghị agwakọta bụ ịbawanye ntinye okpomọkụ na mgbidi akụkụ. N'usoro njikọta laser, enwere ike nweta nkesa ike dị mma nke ogwe laser n'elu ihe eji arụ ọrụ site na ntụgharị ogwe. Mgbe obosara nke oghere ahụ gbanwere, a na-agbanwe oke nke ntụgharị ogwe ka ọ dakọọ obosara nke oghere ahụ, ka o wee mepụta ntinye okpomọkụ dị irè na mgbidi akụkụ.

Igwe ịgbado ọkụ laser

2. Foto macroscopic nke weld site na oyi akwa mbụ (L1) ruo oyi akwa nke asaa (L7) maka ịgbado ọkụ laser nwere ma ọ bụ na-enweghị oscillation.

 

Belata ntụpọ porosity:

Enwere ike ikwu na usoro mgbochi nke laser swing on welding pores bụ ime ka obere oghere kwụsie ike ma melite mmiri mmiri nke metal mmiri. Foto nke 3 na-egosi omume mmiri nke ọdọ mmiri gbazere agbaze nke ihe ndị na-egosi tracer gosiri n'oge usoro ịgbado ọkụ. Mbugharị nke ìhè ọkụ na-eme ka obere oghere ahụ mepụta mmegharị mkpali dị elu na ọsọ ọsọ, nke na-akwalite afụfụ ahụ na-ejupụta ma nwee mmetụta "ọnyà" na pores siri ike. N'otu oge ahụ, mbugharị nke ìhè ọkụ na-eme ka mpaghara obere oghere ahụ dịkwuo elu ma na-ebelata ohere nke ịda ada ya iji mepụta afụ.

Ịdọnye laser 3

3. (a) na (b) ụzọ nke ihe ndị na-egosi ihe n'oge ịgbado ọkụ; Ebe oghere oghere igodo: (c) enweghị laser na-agbanwe agbanwe (d) laser na-agbanwe agbanwe.

Belata ntụpọ mgbawa:

Mgbawa okpomọkụ bụ ụdị ntụpọ e ji mee ihe n'usoro ịgbado ọkụ n'ihi mmekọrịta nke nrụgide dị n'ime na ihe ndị metụtara ígwè, nke a na-ahụkarị na mpaghara ọkụ metụtara (HAZ) nke ịgbado ọkụ. Mmepụta mgbawa ndị dị otú ahụ metụtara adịghị ike nke ihe ahụ na okpomọkụ dị elu, nrụgide ịgbado ọkụ na ihe mejupụtara kemịkalụ nke ihe ahụ. Teknụzụ ịgbado ọkụ laser ọdịnala nwere ike imepụta mgbawa okpomọkụ na usoro ịgbado ọkụ, ọkachasị maka ihe ndị a: Nke mbụ, n'ihi ntinye ike dị elu nke ịgbado ọkụ laser, na-ebute ọkụ ngwa ngwa na oyi nke mpaghara ịgbado ọkụ, na-ebute nnukwu mgbada okpomọkụ na nrụgide okpomọkụ; Nke abụọ, mmeghachi omume metallurgical na usoro ịgbado ọkụ nwere ike ibute nkewa nke ihe ndị na-adịghị ọcha nwere obere ebe ịgbado ọkụ, na-emepụta usoro gbawara agbawa ma na-amụba mmetụta nke mgbawa. N'ikpeazụ, ịgbado ọkụ ngwa ngwa nke ihe ahụ nwere ike ibute ọdịiche nke obere nhazi, na ntụzịaka uto nke kristal kọlụm sitere na ọdọ mmiri gbazere agbaze ruo na etiti, dịka egosiri na Foto 4. N'okwu a, mmetụta maka ịgbado ọkụ na-abawanye nke ukwuu.

Ịkwado laser4

4. Ụdị ịgbado ọkụ laser (a) ịgbado ọkụ laser nkịtị (b) ịgbado ọkụ laser swing.

Teknụzụ ịgbado ọkụ laser nwere ike ibelata ma ọ bụ wepụ ihe mgbawa ọkụ site n'iwebata oghere laser na-agbagharị agbagharị. N'oge usoro ịgbado ọkụ laser na-agbagharị agbagharị, mgbagharị oge nke oghere laser nwere ike ịkwalite usoro ígwè dị n'ọdọ mmiri ahụ gbazere agbaze, si otú a na-eme ka otu nhazi ahụ dịkwuo mma, mkpụrụ ahụ na-etolitekwa coaxial n'etiti ọdọ mmiri ahụ gbazere agbaze, dịka egosiri na Foto 5. Mkpụrụ coaxial ndị a na-arụ ọrụ dị ka ihe mgbochi nchebe iji gbochie mgbasa mgbawa ma na-arụ ọrụ dị ka ihe mkpuchi okpomọkụ iji gbochie mgbasa mgbawa ọzọ. N'otu oge ahụ, laser na-agbagharị agbagharị na-enyere aka belata nhazi nkebi mgbawa n'ihi nkewa nke akụkụ, na-ebelata ihe egwu nke mgbawa okpomọkụ.

Ịkwado laser5

5. (A) njirimara nhazi siri ike nke njikọta njikọta laser nkịtị (B) njirimara nhazi siri ike nke njikọta njikọta laser (CCW).

Ma e jiri ya tụnyere ịgbado ọkụ laser onwe onye, ​​a matala teknụzụ ịgbado ọkụ laser swing dị ka ụzọ dị irè isi belata ohere nke porosity ma melite ntụpọ dịka enweghị njikọ nke mgbidi akụkụ. N'ihi mmetụta mkpali nke osisi ahụ na ọdọ mmiri gbazere agbaze, ọ nwere uru dị ukwuu n'imeziwanye oghere dabara adaba, imeziwanye nha nha microstructure na imeziwanye ọka. Itinye teknụzụ ịgbado ọkụ laser swing nwere ike ime ka a na-ejikarị ịgbado ọkụ laser eme ihe nke ọma, enwere ike nweta ịgbado ọkụ laser nke ọma maka nnukwu ọrụ na ịgbado ọkụ sara mbara, ya bụ, usoro na izi ezi nke ngwaahịa ahụ na-ebelata.